HomeProductsNylon 6 ChipsBright Nylon 6 ChipsLOW VOSCOSITY R.V2.45 NYLON6 RAW MATERIAL

LOW VOSCOSITY R.V2.45 NYLON6 RAW MATERIAL

  • $1.6
    25-24
    Metric Ton
  • $2.5
    ≥25
    Metric Ton
Payment Type:
L/C,T/T,D/P
Incoterm:
FOB,CFR,CIF,EXW
Min. Order:
1 Metric Ton
Transportation:
Ocean,Land,Air
Port:
SHANGHAI,TAICANG,ZHANGJIAGANG
Share:
Chat Now
  • Product Description
Overview
Product Attributes

Model No.HY2000A/HY2500A

BrandQIUXUE

Place Of OriginChina

Types OfSynthetic Resin And Plastics

RELATED VISCOSITY2.45

ColorRaw White

Packing25kgs Or 800kgs Jumbo Bag

Supply Ability & Additional Information

PackagingTHE INNER LAYER IS ALUMINUM FOIL AND THE OUTER LAYER IS PP OR KRAFT BAGS.

Productivity30000 TONS PER MONTY

TransportationOcean,Land,Air

Place of OriginCHINA

Supply Ability350,000 TONS PER YEAR

CertificateISO9000,ISO14001

HS Code390810

PortSHANGHAI,TAICANG,ZHANGJIAGANG

Payment TypeL/C,T/T,D/P

IncotermFOB,CFR,CIF,EXW

Packaging & Delivery
Selling Units:
Metric Ton
Package Type:
THE INNER LAYER IS ALUMINUM FOIL AND THE OUTER LAYER IS PP OR KRAFT BAGS.
Picture Example:

Nylon Pa6 has chemical and physical properties very similar to Nylon 66, but has a lower melting point and a wider processing temperature range. It has better impact and dissolution resistance than Nylon 66 plastic, but is also more hygroscopic. Since many quality properties of plastic parts are affected by hygroscopicity, it is important to take this into account when designing products that use Nylon 6. In order to improve the mechanical properties of nylon 66 materials, various modifiers are usually added. Glass fiber is the most common additive, and synthetic rubbers like EPDM and SBR are sometimes added to improve impact resistance. For products without additives, the shrinkage of nylon 6 plastic materials is between 1% and 1.5%. Adding glass fiber additives reduces shrinkage to 0.3% (but slightly higher perpendicular to the process). Shrinkage of molded components is primarily affected by the crystallinity and hygroscopicity of the material. Actual shrinkage is also a function of part design, wall thickness and other process parameters. Nylon 6 injection drying treatment Since nylon 6 is easy to absorb moisture, special attention should be paid to drying before processing. If the material is supplied in waterproof packaging, the container should be kept tightly closed. If the humidity is greater than 0.2%, it is recommended to dry in hot air above 80°C for 16 hours. If the material is exposed to air for more than 8 hours, vacuum drying at 105°C for more than 8 hours is recommended
Why choose us:
1. We were established in 1970 and have 50 years of experience in the PA 6 field.
2. 1600 employees
3. Our sales exceeded $400 million in 2020
4. We have ISO9000, ISO14001, IATF16949, REACH, ROHS, TFS certificates.
Specification:

NO

ITEM

NORM

DATA

1

VISCOSITY

Q/321200WLB001—2019

M±0.04

2

MONOMER CONTENT(% )

Q/321200WLB001—2019

0.6

3

MOISTURE CONTENT(% )

Q/321200WLB001—2019

≤0.06

4

AMINE END GROUPS(Meg/kg)

Q/321200WLB001—2019

40±3

Dsc 0962 2Bright Pa6 Chips02Dpp 0035

Product Categories : Nylon 6 Chips > Bright Nylon 6 Chips

Company Overview

BRIGHT NYLON6 CHIPS IS WIDELY USED IN ENGINEERING PLASTIC AND TEXTILE GRADE.ITS VISCOSITY IS FROM 2.0 TO 3.45.ITS ADVANTAGE IS GOOD APPEARANCE, GOOD SPINNING ABILITY,HIGH STRENGTH AND HIGH DYEING PERFORMANCE.WE PRODUCE THE PRODUCT VIA HIGH HIGH-END LIQUID MATERIALS WHICH IS IMPORTED FROM USA, JAPAN, THE NETHERLANDS, ETC., WITH VK CONTINUOUS POLYMERIZATION, UNDERWATER GRANULATION, CONTINUOUS AIRFLOW DRYING, DCS CONTROL AND OTHER TECHNOLOGIES.THE AMINO TERMINAL GROUP, MONOMER CONTENT AND OTHER SPECIFICATION ARE BETTER.

 

WHY CHOOSE US:

1. WE ESTABLISH IN 1970,WITH 50 YEARS’ EXPERINCE IN PA6 FIELD.

2. 1600 EMPLOYEE

3. OUR SALES AMOUNT IN 2020 IS MORE THAN USD400.00 MILLION

4. WE HAVE ISO9000,ISO14001,IATF16949,REACH,ROHS,TFS CERTRIFICATE.

SPECIFICATION:

NO

ITEM

NORM

DATA

1

VISCOSITY

Q/321200WLB001—2019

M±0.04

2

MONOMER CONTENT(% )

Q/321200WLB001—2019

0.6

3

MOSITURE CONTENT(% )

Q/321200WLB001—2019

≤0.06

4

AMINE END GROUPS(Meg/kg)

Q/321200WLB001—2019

40±3

Company Photos
Production Certification
Email to this supplier
  • *Subject:
  • *To:
    Mr. bill han
  • *Email:
  • *Message:
    Your message must be between 20-8000 characters
HomeProductsNylon 6 ChipsBright Nylon 6 ChipsLOW VOSCOSITY R.V2.45 NYLON6 RAW MATERIAL
Send Inquiry
*
*

Related Products List

Home

Product

Whatsapp

About Us

Inquiry

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send